Polymer Property : Charpy Impact, Notched = 9.50 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 1.20 - 9.50 J/cm²
5.71 - 45.2 ft-lb/in²
Average value: 4.64 J/cm² Grade Count:7
Overview of materials for Polycarbonate, Gamma Radiation Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum..