Izod Impact, Notched | 0.153 - 0.241 J/cm | 0.287 - 0.451 ft-lb/in | Average value: 0.187 J/cm Grade Count:25 |
Overview of materials for Phenolic, Novolac, Woodflour Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Woodflour Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.153 J/cm | 0.287 ft-lb/in | ASTM D256 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Izod Impact, Notched | 0.153 J/cm | 0.287 ft-lb/in | ASTM D256 |
Plenco 4301 Phenolic, Granular, Compression Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |