Polymer Property : Izod Impact, Notched = 0.192 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.192 J/cm
0.360 ft-lb/in
X, Y direction; ASTM D256A
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite
TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope..
Izod Impact, Notched 0.192 J/cm
0.360 ft-lb/in
ASTM D256
Plenco 7523 Phenolic, Granular, Transfer Molded
PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P..
Izod Impact, Notched 0.192 J/cm
0.360 ft-lb/in
ASTM D256
Ensinger TECACRYL®
TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to cr..