Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.192 J/cm | 0.360 ft-lb/in | X, Y direction; ASTM D256A |
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Izod Impact, Notched | 0.192 J/cm | 0.360 ft-lb/in | ASTM D256 |
Plenco 7523 Phenolic, Granular, Transfer Molded PLENCO 07523 is a woodflour and cotton flock filled novolac phenolic molding compound, formulated for high impact industrial uses. UL recognized under component file E40654.Information supplied by P.. |
|||
Izod Impact, Notched | 0.192 J/cm | 0.360 ft-lb/in | ASTM D256 |
Ensinger TECACRYL® TECACRYL® offers excellent weather resistance, high light transmission, high mechanical strength, high surface hardness and mar resistance, good melt flow rate, and versatile colorability due to cr.. |