Polymer Property : Izod Impact, Notched = 0.236 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.236 J/cm
0.442 ft-lb/in
ASTM D256-06
Objet FullCure® 840 Vero Blue Resin for Rapid Prototyping
Information provided by American Precision Prototyping, LLC
Izod Impact, Notched 0.236 J/cm
0.442 ft-lb/in
ASTM D256
Plenco 4414 Phenolic, Granular, Transfer Molded
PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional ..