Mechanical Properties Metric English Comments
Izod Impact, Notched 0.168 J/cm
0.315 ft-lb/in
ASTM D256
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Izod Impact, Notched 0.168 J/cm
0.315 ft-lb/in
ASTM D256
Plenco 00732 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00732 is a melamine-phenolic copolymer molding compound, exhibiting excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 007..
Izod Impact, Notched 0.168 J/cm
0.315 ft-lb/in
ASTM D256
Plenco 3356 Phenolic, Granular, Injection Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..