Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.171 J/cm | 0.320 ft-lb/in | ASTM D256 |
Plenco 4548 Phenolic, Granular, Transfer Molded PLENCO 04548 is a heat resistant mineral filled phenolic molding compound, offering fast cure rates and hot rigidity. Type ASTM 5948 CFG, and UL recognized under component file E40654. 04548 is avai.. |
|||
Izod Impact, Notched | 0.171 J/cm | 0.320 ft-lb/in | ASTM D256 |
Plenco 4504 Phenolic, Granular, Injection Molded Plenco 04504 is a renumber of Plaslok 504. Plenco 04504 is a two-stage, mineral and cellulose-filled phenolic molding compound having better impact and heat resistance than general purpose molding c.. |
|||
Izod Impact, Notched | 0.171 J/cm | 0.320 ft-lb/in | 90 Minute UV Cure; SLA 3500 System; ASTM D256 |
3D Systems Accura® accuGen™ Nd Plastic for SLA® Systems Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® Viper si2™, 3500, 5000 & 7000 systems.Typical ApplicationsMulti-purpose mode.. |