Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.358 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.670 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Therma-Tech™ PI-5000 TC Polyetherimide (PEI)