Polymer Property : Izod Impact, Notched = 0.363 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.363 J/cm
0.680 ft-lb/in
Abatron AboCast 8-8/Abocure 8-8 Epoxy  (discontinued **)
2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 135 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F)...
Izod Impact, Notched 0.363 J/cm
0.680 ft-lb/in
ASTM D256
Kolon DIAMAT® EM
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Izod Impact, Notched 0.363 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.680 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical Lupox® GP1000A PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Izod Impact, Notched 0.363 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.680 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical Lupox® GP1000D PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Izod Impact, Notched 0.363 J/cm
0.680 ft-lb/in
ASTM D256
E-Polymers SEPAZ® V230B 30% Mineral Filled Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Izod Impact, Notched 0.363 J/cm
0.680 ft-lb/in
Abatron AboCast 50-16/AboCure 50-17 Epoxy
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/28 ratio. Pot life: 500 g, 29 min. at 70°C (160°F). Exothermic Peak 242°C (468°F). Cures in 1-2 hrs at ..