Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.379 J/cm | 0.710 ft-lb/in | ASTM D256 |
Custom Resins Duratel™ MF27 Acetal Copolymer
(discontinued **) Description: Duratel™ MF27 is a 27 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Izod Impact, Notched | 0.379 J/cm @Temperature 23.0 °C |
0.710 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |
|||
Izod Impact, Notched | 0.379 J/cm | 0.710 ft-lb/in | ASTM D256 |
ExxonMobil HDPE HPA 020 Molding High Density Polyethylene (HMW) Resin Product Description: HPA 020 is a high molecular weight HDPE resin, characterized by excellent balance of rigidity, ESCR and impact strength. Availability: Africa & Middle East, Asia Pacific and Eur.. |
|||
Izod Impact, Notched | 0.379 J/cm | 0.710 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336M10CL Mica Reinforced Coupled |
|||
Izod Impact, Notched | 0.379 J/cm | 0.710 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0336M30L Mica Reinforced |