Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.233 - 0.470 J/cm | 0.437 - 0.881 ft-lb/in | Average value: 0.364 J/cm Grade Count:3 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.233 J/cm | 0.437 ft-lb/in | ASTM D256 |
Plenco 7487 Phenolic, Granular, Transfer Molded PLENCO 07487 is a rubber modified organic reinforced phenolic molding compound offering improved mechanical strength and lower modulus. Plenco 07487 is available in black.Information supplied by Ple.. |