Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.233 - 0.470 J/cm | 0.437 - 0.881 ft-lb/in | Average value: 0.364 J/cm Grade Count:3 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 0.450 - 0.470 J/cm @Temperature -40.0 - -20.0 °C |
0.843 - 0.881 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.460 J/cm Grade Count:1 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |