Izod Impact, Notched 0.241 J/cm
0.451 ft-lb/in
ASTM D256-06
Objet FullCure® 830 Vero White Resin for Rapid Prototyping
Information provided by American Precision Prototyping, LLC
Izod Impact, Notched 0.241 J/cm
0.451 ft-lb/in
ASTM D256
Plenco 1508 Polyester, Briquette, Transfer Molded
PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is availabl..
Izod Impact, Notched 0.241 J/cm
0.451 ft-lb/in
ASTM D256
Plenco 7579 Phenolic, Granular, Compression Molded
PLENCO 07579 is a fast curing, woodflour filled, novolac phenolic molding compound, formulated for industrial applications that do not require a smooth finish. UL recognized under component file E40..