Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.262 J/cm | 0.490 ft-lb/in | ASTM D256 |
Ensinger Tecatron® XP-84 Compression Molded PPS Compound, 30% Graphite Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Izod Impact, Notched | 0.262 J/cm | 0.490 ft-lb/in | |
Atom Adhesives AA-SUPERTHERM 05 Epoxy Adhesive AA-SUPERTHERM 05 is a thixotropic (smooth paste) Pure Diamond ultra-high thermally conductive epoxy two-part adhesive that develops strong, durable, high-impact bonds at room temperature which impro.. |
|||
Izod Impact, Notched | 0.262 J/cm @Temperature 22.8 °C |
0.490 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene CPP1040 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 40% Filler by Weight Features: Homopolymer Uses: Appliance Components; Furniture; Housings F.. |
|||
Izod Impact, Notched | 0.262 J/cm | 0.490 ft-lb/in | |
Abatron AboCast/AboCure 7606-1 Epoxy AboCast 7606-1 is a transparent, light amber resin with a weight of 9.5 lbs/gallon and a viscosity of 2100 cps approx. @ 25°C. AboCure 7606-1 is a transparent, light amber converter with a weight o.. |