Abatron AboCast/AboCure 7606-1 Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast/AboCure
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast/AboCure 7606-1 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 7606-1 is a transparent, light amber resin with a weight of 9.5 lbs/gallon and a viscosity of 2100 cps approx. @ 25°C. AboCure 7606-1 is a transparent, light amber converter with a weight of 7.9 lbs/gallon and a viscosity of 500 cps approx. @ 25°C. AboCast/AboCure 7606-1 is a 2-component, dielectric, variable-ratio low-viscosity plasticized epoxy system. It is a clear dielectric casting, adhesive, and encapsulation compound. It is virtually unaffected by atmospheric conditions, soft and salt water, alkalis and diluted acids, several solvents, detergents, oils and greases. Final properties can be controlled by changing the AboCast/AboCure ratios: the highest rigidity, hardness, chemical, and heat resistance are offered by a 100/40 ratio. Higher AboCure ratios (up to 100/100 AboCast/AboCure) yield increasing flexibility, shock and thermocycling resistance, and adhesion to problem surfaces. It has tenacious adhesion to metals, ceramics, wood, fiberglass, masonry, and most materials to form permanent structural and dielectric bonds. Radiation resistance recommends the 7606-1 System in X-ray and other radioactive environments. Other Suggested Uses: Dielectric encapsulation and potting of electronic components, especially where toughness, transparency, mild reactivity, and non-critical proportioning are required; Shrink-free embedments and preparations of specimens for display or analytical purposes; General purpose adhesion, casting, and impregnation; Bonding or laminating substrates, plate, radiation screens, and other components in radioactive equipment.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
AboCure 7606-1
1.14 g/cc
0.0411 lb/in³
AboCast 7606-1
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
AboCast/AboCure ratio: 100/80 pbw
64
64
AboCast/AboCure ratio: 100/100 pbw
70
70
AboCast/AboCure ratio: 100/40 pbw
55

@Time 10.0 sec
55

@Time 0.00278 hour
AboCast/AboCure ratio: 100/100 pbw
62

@Time 10.0 sec
62

@Time 0.00278 hour
AboCast/AboCure ratio: 100/80 pbw
Tensile Strength at Break 51.0 MPa
7400 psi
Flexural Strength 82.7 MPa
12000 psi
Compressive Strength 101 MPa
14600 psi
Izod Impact, Notched 0.262 J/cm
0.490 ft-lb/in
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 60.0 - 180 min

@Temperature 80.0 - 110 °C
1.00 - 3.00 hour

@Temperature 176 - 230 °F
4320 - 11520 min

@Temperature 20.0 °C
72.0 - 192.0 hour

@Temperature 68.0 °F
(3-8 Days)
Pot Life 16 - 24 min

@Temperature 60.0 - 80.0 °C
16 - 24 min

@Temperature 140 - 176 °F
150 - 180 min

@Temperature 20.0 - 25.0 °C
150 - 180 min

@Temperature 68.0 - 77.0 °F
Descriptive Properties Value Comments
Hardening Time (min) 180-480
Parts by Weight (pbw) 100
AboCast
43
AboCure