Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.271 J/cm | 0.508 ft-lb/in | ASTM D256 |
Plenco 4527 Phenolic, Granular, Transfer Molded PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under.. |