Mechanical Properties Metric English Comments
Izod Impact, Notched 0.0801 - 0.534 J/cm
0.150 - 1.00 ft-lb/in
Average value: 0.191 J/cm Grade Count:51
Overview of materials for Polystyrene, Transparent Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 0.340 - 0.534 J/cm
0.637 - 1.00 ft-lb/in
Average value: 0.469 J/cm Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Izod Impact, Notched 0.157 - 0.534 J/cm
0.294 - 1.00 ft-lb/in
Average value: 0.280 J/cm Grade Count:13
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched 0.427 - 0.534 J/cm

@Temperature 22.8 °C
0.800 - 1.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Ensinger TECAST™ Cast Nylon (PA)
TECAST™ Cast Nylon reduces downtime in heavy equipment applications. It is a low cost alternative for many non-ferrous machined parts. It has self-lubricating qualities which provide for excellen..
Izod Impact, Notched 0.427 - 0.534 J/cm

@Temperature 22.8 °C
0.800 - 1.00 ft-lb/in

@Temperature 73.0 °F
Ensinger TECAST VEKTON™ 6PB Nylon 6 (PA6)
TECAST VEKTON™ 6PB cushion pads are used to dampen the shock load on the anvil of a pile hammer. Specially formulated from an impact-modified type 6 nylon, they combine the excellent strength of n..
Izod Impact, Notched 0.427 - 0.534 J/cm
0.800 - 1.00 ft-lb/in
ASTM D256
Aaron Industries AAROLENE® ARPP H 200-1 Polypropylene Compounded Resin
AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified.
Izod Impact, Notched 0.427 - 0.534 J/cm
0.800 - 1.00 ft-lb/in
ASTM D256
Aaron Industries AAROLENE® ARPS GP 100-1 Polystyrene Compounded Resin
AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified.
Izod Impact, Notched 0.267 - 0.534 J/cm
0.500 - 1.00 ft-lb/in
Average value: 0.450 J/cm Grade Count:7
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched 0.200 - 0.534 J/cm
0.375 - 1.00 ft-lb/in
Average value: 0.276 J/cm Grade Count:7
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
Izod Impact, Notched 0.427 - 0.534 J/cm
0.800 - 1.00 ft-lb/in
Average value: 0.494 J/cm Grade Count:4
Overview of materials for Acrylic, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched 0.427 - 0.534 J/cm
0.800 - 1.00 ft-lb/in
Average value: 0.498 J/cm Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved