Mechanical Properties Metric English Comments
Izod Impact, Notched 0.336 J/cm
0.630 ft-lb/in
ASTM D256
Ensinger Tecatron® XP-72 Compression Molded PPS Compound, 20% PTFE Filled Natural
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..