Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecatron® XP-72 Compression Molded PPS Compound, 20% PTFE Filled Natural

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with PTFE Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-72 Compression Molded PPS Compound, 20% PTFE Filled Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Filler Content 64 %
64 %
Mechanical Properties Metric English Comments
Tensile Strength 14.5 MPa
2100 psi
ASTM D638
Elongation at Break 1.3 %
1.3 %
ASTM D638
Tensile Modulus 2.83 GPa
410 ksi
ASTM D638
Flexural Strength 24.1 MPa
3500 psi
ASTM D790
Flexural Modulus 1.79 GPa
260 ksi
ASTM D790
Compressive Strength 24.1 MPa
3500 psi
ASTM D695
Izod Impact, Notched 0.336 J/cm
0.630 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Color Dark Brown