Polymer Property : Izod Impact, Notched = 0.637 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.250 - 0.340 J/cm

@Thickness 6.35 mm
0.468 - 0.637 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chang Chun Plastic PBT2000 Fire Retardant PBT
Information provided by Dowell Trading Company Ltd.
Izod Impact, Notched 0.250 - 0.340 J/cm

@Thickness 6.35 mm
0.468 - 0.637 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chang Chun Plastic PBT2100 Fire Retardant PBT
Information provided by Dowell Trading Company Ltd.