Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.250 - 0.350 J/cm | 0.468 - 0.656 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Izod Impact, Notched | >= 0.250 J/cm @Temperature 23.0 °C |
>= 0.468 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 1500P (V30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Izod Impact, Notched | 0.250 - 6.41 J/cm | 0.468 - 12.0 ft-lb/in | Average value: 1.05 J/cm Grade Count:69 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature -30.0 °C |
0.468 ft-lb/in @Temperature -22.0 °F |
ASTM D256A |
Total Finaclear® 520 Clear Impact Polystyrene
(discontinued **) Finaclear® 520 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles. Complemented by inherent repr.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature -30.0 °C |
0.468 ft-lb/in @Temperature -22.0 °F |
ASTM D256A |
Total Finaclear® 521 Clear Impact Polystyrene
(discontinued **) Finaclear® 521 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with othe.. |
|||
Izod Impact, Notched | 0.250 - 5340 J/cm | 0.468 - 10000 ft-lb/in | Average value: 3.49 J/cm Grade Count:74 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | |
Cookson Group Plaskon® 3100 Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A flame retardant, novolac-hardened epoxy molding compound recommended for semiconductor packages that are not stress sensitive. |
|||
Izod Impact, Notched | 0.250 J/cm - NB | 0.468 ft-lb/in - NB | Average value: 2.26 J/cm Grade Count:17 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched | 0.250 - 2.60 J/cm | 0.468 - 4.87 ft-lb/in | Average value: 0.673 J/cm Grade Count:24 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for .. |
|||
Izod Impact, Notched | 0.250 - 0.300 J/cm @Temperature -40.0 - -20.0 °C |
0.468 - 0.562 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.275 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Mitsui APELâ„¢ APL6015T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
JPJ Technologies PP HC9012-M PP Homopolymer Injection Molding Information provided by JPJ Technologies |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON AD000 ABS LNP* STAT-KON* AD000 is a compound based on ABS containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP M7001XXH PP LNP* THERMOCOMP* M7001XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additves. Designed for touch surfaces in patient critical healthcare applications. Added f.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 3000-3120 Glass Sphere Filled Copolymer Polypropylene DescriptionPolyfort® FXP 3000-3120 is a 30% glass sphere filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Goodfellow TPX® DX310 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene Description: SHA7260 is a high-density polyethylene, developed for the injection molding, easy to process and with high productivity. This resin has a good melt flow with high rigidity and hardness... |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature 23.0 °C |
0.468 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 103 Injection Molding Polypropylene Applications: Thin-walled parts and easy mould filling; food and cosmetic packing; toys and household; sealed closures. Information provided by Braskem |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM-D256 |
Braskem H 216 HOMO Polypropylene Homopolymer H 216 is a high melt flow rate homopolymer with narrow molecular weight distribution. It is designed for fiber extrusion processing with high toughness fibers. H 216 exhibits excellent processabilit.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature >=23.0 °C |
0.468 ft-lb/in @Temperature >=73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® T 12 EV Polypropylene Homopolymer CAPILENE® T 12 EV is a polypropylene homopolymer with narrow molecular weight distribution, controlled rheology, intended for fiber applications. It is characterized by easy processing, very good m.. |
|||
Izod Impact, Notched | 0.250 J/cm @Temperature >=23.0 °C |
0.468 ft-lb/in @Temperature >=73.4 °F |
ASTM D256 |
Carmel Olefins CAPILENE® T 77 A Polypropylene Homopolymer CAPILENE® T 77 A is a high melt flow rate polypropylene homopolymer for injection molding with nucleation and antistatic additivation. It exhibits good stiffness, combined with good thermal stabili.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Carmel Olefins CAPILENE® U 77 A Polypropylene Homopolymer Description: CAPILENE® U 77 A is a high melt flow rate homopolymer for injection molding of products with long flow length. It is specially formulated with antistatic and nucleating additives, al.. |
|||
Izod Impact, Notched | 0.250 - 0.400 J/cm | 0.468 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATO 142 Phenolic Molding Organic Filler, Compression Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-black, brownMedium/hard flow Applications: Elec.. |
|||
Izod Impact, Notched | 0.250 - 0.400 J/cm | 0.468 - 0.749 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Izod Impact, Notched | 0.250 - 0.300 J/cm | 0.468 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa.. |
|||
Izod Impact, Notched | 0.250 J/cm | 0.468 ft-lb/in | ASTM D256 |
Plenco 301 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 301 is a two-stage, woodflour and flock-filled phenolic molding compound. It has broad molding latitude combined with good electrical properties and improved impact strength. It is particu.. |
|||
Izod Impact, Notched | 0.250 - 1.35 J/cm @Diameter 0.125 - 3.17 mm |
0.468 - 2.53 ft-lb/in @Diameter 0.00492 - 0.125 in |
Average value: 0.794 J/cm Grade Count:11 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.250 - 6.00 J/cm | 0.468 - 11.2 ft-lb/in | Average value: 0.723 J/cm Grade Count:95 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |