Mechanical Properties Metric English Comments
Izod Impact, Notched 0.660 J/cm

@Temperature 23.0 °C
1.24 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Mytex Polymers AS14KW-02 Polypropylene, Talc filled, Compounded
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym..
Izod Impact, Notched 0.660 J/cm

@Temperature -30.0 °C
1.24 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific)
Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD.
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
Covestro Petlon® DP3-1042 Semi-Crystalline PET, 40% Mineral/Glass Fiber  (discontinued **)
Characteristics: General Purpose: Good Strength and Dimensional Stability, Low WarpageApplications: Automotive Valve Covers, Pump Components and PulleysProcessing: Injection Molding (Melt Temperatur..
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
Plenco 50030 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256A
LyondellBasell Pro-fax SR549M Polypropylene Random Copolymer, Clarified
Primary Processing Method: Injection Molding and Injection Stretch Blow MoldingKey Features: clarified polypropylene random copolymer resin, superior clarity, good impact and rigidity balance, good ..
Izod Impact, Notched 0.660 J/cm

@Temperature 23.0 °C
1.24 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified
Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi..
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI
LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66
LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized.
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP SH0430AC_BK1D466 PA12
4.3 specific gravity nylon 12, clean compound system
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP SH0700B PA12
LNP* Thermocomp* SH0700B is a compound based on Nylon 12 containing proprietary fillers. Added feature: High Specific Gravity
Izod Impact, Notched 0.660 J/cm

@Temperature -30.0 °C
1.24 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL PX300 PPE+HIPS (Asia Pacific)
Low odor grade for IC tray application
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP EP003 PEI
LNP* Lubricomp EP003 is a Polyetherimide containing 15% PTFE/Silicone. Added features include: Internally Lubricated.
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC (Asia Pacific)
LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
UBE B (Low-Cis) HIPS (n-DM =0.03 wt %)
Description: UBE high impact polystyrene (HIPS).Information provided by UBE.
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
Plenco 51030 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 51030 is an engineering grade glass reinforced recycled polyethylene terephthalate resin designed for good physical strength. It is UL listed.Information supplied by PlencoPlenco discontinued..
Izod Impact, Notched 0.660 J/cm

@Temperature -40.0 °C
1.24 ft-lb/in

@Temperature -40.0 °F
ISO 180
LyondellBasell Hifax™ ETA-3163 Thermoplastic Olefin Resin
Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good dimensional stability, good paintability, good pro..
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10
LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant.