SABIC Innovative Plastics LNP STAT-KON 9X02785 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON 9X02785 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 2.89 GPa
419 ksi
50 mm/min; ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 2.89 GPa
419 ksi
ASTM D790
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256
Izod Impact, Unnotched 16.02 J/cm
30.01 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C

@Thickness 3.20 mm
216 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+7 ohm-cm
100 - 1.00e+7 ohm-cm
ASTM D257
Surface Resistance 100 - 1.00e+7 ohm
100 - 1.00e+7 ohm
ASTM D257