Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.402 - 1.23 J/cm | 0.753 - 2.30 ft-lb/in | Average value: 0.681 J/cm Grade Count:45 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |