Polymer Property : Izod Impact, Notched = 0.955 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.510 J/cm

@Thickness 3.18 mm,
Temperature -40.0 °C
0.955 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
Compression Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 0.510 J/cm

@Temperature 23.0 °C
0.955 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Mytex Polymers AS33L-07VS Polypropylene, Rubber modified, Compounded
Description: AS33L-07 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key..
Izod Impact, Notched 0.510 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.955 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
PolyOne Geon™ HTX L1502 Polyvinyl Chloride Alloy (PVC Alloy)
Physical properties based on Geon HTX L1502 white 1000.Information provided by PolyOne
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer
LNP LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing 15% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Low Extractable.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR
LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
63.5*12.7*3.2mm, Cut; ASTM D256
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP
SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold..
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP RAL22I PA 66
LNP* LUBRICOMP* RAL22I is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant, High Impact.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66
LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
Izod Impact, Notched 0.510 J/cm

@Temperature -30.0 °C
0.955 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East)
VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET
LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS
LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s).
Izod Impact, Notched 0.510 J/cm

@Temperature 23.0 °C
0.955 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC
LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the..
Izod Impact, Notched 0.510 J/cm

@Temperature -40.0 °C
0.955 ft-lb/in

@Temperature -40.0 °F
ASTM Test
Styrolution Luran® S 776 SE ASA
Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between ..
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP MF006AS PP
LNP THERMOCOMP* MF006AS is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT
LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific)
Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
UBE C (Low-Cis) HIPS (n-DM = 0.03 wt % and PH-3H = 0.03 wt %)
Description: UBE high impact polystyrene (HIPS).Information provided by UBE.
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
Cheng Yu Plastic PP236G1 Polypropylene, 10% Glass Fiber
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
E-Polymers TEKAPPO® JF201 Filler Reinforced Heat Resistant Dimensional Stability Flame Retardant M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Izod Impact, Notched 0.510 J/cm
0.955 ft-lb/in
ASTM D256
Plenco 50335 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform..