Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
15 sec; ASTM D2240
Tensile Strength, Yield 50.5 MPa
7320 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.83 GPa
410 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 104 MPa
15100 psi
ASTM D790
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Izod Impact, Notched 0.510 J/cm

@Thickness 3.18 mm,
Temperature -40.0 °C
0.955 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy 62.3 J/cm

@Temperature 23.0 °C
0.117 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
133 J/cm

@Temperature 23.0 °C
0.249 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.0 µm/m-°C
28.9 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C

@Thickness 3.18 mm
158 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Agency Ratings NSF 51
NSF Type I
Ease of Sizing Good
Features Good Chemical Resistance
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
PVC Cell Classification 12454
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Piping
Users viewing this material also viewed the following: