Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.603 J/cm @Temperature 23.0 °C |
1.13 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Forte™ 18CPP091 Nanocomposite Forte is a polypropylene-based nanocomposite produced by Noble Polymers. It is one of the first commercialization of nanocomposites in the automotive industry and can be used in a variety of applica.. |
|||
Izod Impact, Notched | 0.603 J/cm @Temperature -40.0 °C |
1.13 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
ExxonMobil HD 6714.17 Injection Molding Resin
(discontinued **) HD 6714 is a narrow molecular weight hexene copolymer designed for outstanding processability to maximize injection molding productivity. This resin is ideally suited for thin wall multicavity part.. |
|||
Izod Impact, Notched | 0.603 J/cm @Thickness 3.17 mm |
1.13 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® FPI-15 BK Nylon 6, 15% Glass Reinforced, post industrial Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.603 J/cm | 1.13 ft-lb/in | ASTM D256 |
Ineos R35C-02 Polypropylene Random Copolymer Grade R35C-02 is a high clarity, lubricated random copolymer with a high flow rate. This material is designed for high-speed injection molding of medium- to thin-walled parts requiring excellent cla.. |
|||
Izod Impact, Notched | 0.603 J/cm | 1.13 ft-lb/in | ASTM D256 |
Cheng Yu Plastic A707G25 SAN, 25% Glass Fiber |