Material Notes:
Information provided by FIBERFIL Engineered Plastics
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Flexural Strength 171 MPa
24800 psi
ASTM D790
Flexural Modulus 4.90 GPa
711 ksi
Secant; ASTM D790
Izod Impact, Notched 0.603 J/cm

@Thickness 3.17 mm
1.13 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
ASTM D648