Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. This resin has thinwall FR capability and has a UL94 V0 listing. Resin is RoHS compliant and halogen free acc.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS (Europe-Africa-Middle East) LNP* Faradex* NS003 is a compound based on PC+ABS Blend resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
Kolon KOPA® KN3321G10V0L G/F Reinforced & Flame Retardant Nylon 66 High flame resistant, high toughness, dimensionally stableApplications A variety of connectorsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66 LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5211R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12 LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS (Asia Pacific) LNP* Thermocomp* AF003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific) LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF0046P PC (Asia Pacific) LNP* Thermocomp* DF0046P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Exceptional Processing, Flame Retardant, Non-Br.. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC LNP THERMOCOMP* DF004P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature 23.0 °C |
1.39 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp DX99721 PC (Asia Pacific) LNP* Thermocomp* DX99721 is a compound based on Polycarbonate resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 LNP* THERMOCOMP* IC006 is a compound based on Nylon 6/12 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP LNP* THERMOCOMP* MX99432 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP OC006 PPS - Linear (Asia Pacific) LNP* Thermocomp* OC006 is a compound based on PPS - Linear resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069S PA 66 LNP THERMOCOMP* RF0069S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP ZF0089 PPE+PS LNP* THERMOCOMP* ZF0089 is a compound based on PPE+PS resin containing 40% Glass Fiber. Added features of this material include: Exceptional Processing, Flame Retardant. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature 23.0 °C |
1.39 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC (Asia Pacific) LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supp.. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature -30.0 °C |
1.39 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Izod Impact, Notched | 0.740 J/cm | 1.39 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MX99432 PP (Asia Pacific) LNP* Thermocomp* MX99432 is a compound based on Polypropylene resin containing Glass Fiber. |
|||
Izod Impact, Notched | 0.740 J/cm @Temperature 23.0 °C |
1.39 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser.. |