Mechanical Properties Metric English Comments
Izod Impact, Notched 1.08 - 1.40 J/cm
2.02 - 2.62 ft-lb/in
Average value: 1.29 J/cm Grade Count:4
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Izod Impact, Notched 0.160 - 1.40 J/cm
0.300 - 2.62 ft-lb/in
Average value: 0.644 J/cm Grade Count:24
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..