Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Izod Impact, Notched | 1.08 J/cm @Temperature -30.0 °C |
2.02 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched | 1.08 J/cm @Temperature -30.0 °C |
2.02 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Izod Impact, Notched | 1.08 J/cm @Temperature 23.0 °C |
2.02 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Izod Impact, Notched | 1.08 J/cm @Temperature 23.0 °C |
2.02 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARPEEK 50 G/40 40% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLDM310 PC (Asia Pacific) Mineral filled Antistatic Polycarbonate, HDT110degC type |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Izod Impact, Notched | 1.08 - 1.40 J/cm | 2.02 - 2.62 ft-lb/in | Average value: 1.29 J/cm Grade Count:4 |
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66 High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66 EG-resistant, high strength, dimensionally stableApplications Coolant temperature control partsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 1.08 J/cm @Temperature 23.0 °C |
2.02 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC T3410 Polypropylene Random Terpolymer Features: Seetec T3410 is a polypropylene-ethylene-butene random terpolymer designed for the production of Transparent Film and Expandable PP for low seal temperature and high impact strength. It of.. |
|||
Izod Impact, Notched | 1.08 J/cm @Temperature 23.0 °C |
2.02 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® PDR4911 PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | |
Shinil Chemical SHINSTRA PA-6 AG30N Structural Polymer Wheel Cover SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Izod Impact, Notched | 1.08 J/cm @Thickness 3.17 mm |
2.02 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HR-8070 MPPE, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.08 J/cm @Thickness 3.17 mm |
2.02 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SF-0950S MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.08 J/cm @Thickness 3.17 mm |
2.02 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HR-8070 MPPE, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.08 J/cm @Thickness 3.17 mm |
2.02 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR PC/GF material with 40% GF reinforcement that can be used in printer LSUInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.08 J/cm @Thickness 3.17 mm |
2.02 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SF-0950 MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.08 J/cm @Thickness 3.17 mm |
2.02 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® SF-0950S MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | |
Zylog Hipolyene® 5131 SX-5 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
Cheng Yu Plastic ML3420 PC, 20% Glass Fiber |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
Cheng Yu Plastic ML848 Flame Retardant PC |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
E-Polymers TEKAPPO® J920 20% Glass Fiber Reinforced M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
E-Polymers TEKAPPO® JF2 Un-Reinforced Heat Resistant Chemical Resistance M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
E-Polymers TEKASTER® F615G55 55% Glass Fiber Reinforced High Modulus PET Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Izod Impact, Notched | 1.08 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.02 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi.. |
|||
Izod Impact, Notched | 1.08 J/cm | 2.02 ft-lb/in | ASTM D256 |
Plenco 50045 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |