Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.828 J/cm @Thickness 3.17 mm |
1.55 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Oxford Polymers PC 30CF-925 Black PC, 30% Carbon Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents Special Characteristics: High Str.. |
|||
Izod Impact, Notched | 0.830 J/cm | 1.55 ft-lb/in | |
Shell Carilon® DB6G3A10 Polyketone, 15% Glass-Reinforced General-Purpose Injection Molding Grade
(discontinue Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G3A10 is a 15 percent short glass-fiber-reinforced general-purpose injection molding grade with .. |
|||
Izod Impact, Notched | 0.830 J/cm | 1.55 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY RF203H PA 66 LNP LUBRILOY* RF203H is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 0.830 J/cm | 1.55 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY RF203XXH PA 66 LNP* LUBRILOY* RF203XXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 0.830 J/cm @Temperature -30.0 °C |
1.55 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Notched | 0.830 J/cm @Temperature -30.0 °C |
1.55 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Izod Impact, Notched | 0.830 J/cm @Temperature -30.0 °C |
1.55 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Izod Impact, Notched | 0.830 J/cm @Temperature -30.0 °C |
1.55 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Izod Impact, Notched | 0.830 J/cm @Temperature -30.0 °C |
1.55 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Izod Impact, Notched | 0.830 J/cm @Temperature -30.0 °C |
1.55 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ420HP PBT Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Izod Impact, Notched | 0.830 J/cm @Temperature -30.0 °C |
1.55 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Europe-Africa-Middle East) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Izod Impact, Notched | 0.830 J/cm @Temperature 0.000 °C |
1.55 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Izod Impact, Notched | 0.830 J/cm | 1.55 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF VF006U Super Tough Nylon LNP* Thermotuf* VF006U is a compound based on Super Tough Nylon containing Glass Fiber. Characteristics of this grade are High Impact. |
|||
Izod Impact, Notched | 0.830 J/cm | 1.55 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Izod Impact, Notched | 0.830 J/cm | 1.55 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
Izod Impact, Notched | 0.828 J/cm | 1.55 ft-lb/in | ASTM D256 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) Tecapeek™, made from Victrex PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance.Excellent flex.. |
|||
Izod Impact, Notched | 0.828 J/cm @Temperature 22.8 °C |
1.55 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger Tecapeek® Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Izod Impact, Notched | 0.830 J/cm | 1.55 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |