SABIC Innovative Plastics LNP LUBRILOY RF203XXH PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Lubriloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRILOY RF203XXH PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRILOY* RF203XXH is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
1.13 g/cc
0.0408 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 87.0 MPa
12600 psi
Type I, 5 mm/min; ASTM D638
90.0 MPa
13100 psi
5 mm/min; ISO 527
Elongation at Break 3.7 %
3.7 %
Type I, 5 mm/min; ASTM D638
3.8 %
3.8 %
5 mm/min; ISO 527
Tensile Modulus 4.89 GPa
709 ksi
5 mm/min; ASTM D638
Flexural Strength 128 MPa
18600 psi
1.3 mm/min, 50 mm span; ASTM D790
140 MPa
20300 psi
ISO 178
Flexural Modulus 4.18 GPa
606 ksi
1.3 mm/min, 50 mm span; ASTM D790
5.50 GPa
798 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.830 J/cm
1.55 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.46 J/cm
12.1 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.36
0.36
ASTM D3702 Modified
Coefficient of Friction, Static 0.30
0.30
ASTM D3702 Modified
K (wear) Factor 141 x 10-8 mm³/N-M
70.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 232 °C
450 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af