Izod Impact, Notched 0.550 - 0.834 J/cm
1.03 - 1.56 ft-lb/in
Average value: 0.714 J/cm Grade Count:3
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..