Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML3729 PC Excellent flow, UV stabilized, grade which contains a release agent to ensure easy processing. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ISO 180 |
Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade
(discontinued **) Contains PTFE lubricant. Used for injection molding of high performance parts. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Izod Impact, Notched | >= 0.550 J/cm @Temperature 23.0 °C |
>= 1.03 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 8340S (EPYH31U) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.550 J/cm @Diameter 3.17 mm, Temperature -20.0 °C |
1.03 ft-lb/in @Diameter 0.125 in, Temperature -4.00 °F |
bar; ASTM D256 |
BP Amoco Acctuf® 3243 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N145-AS Antistatic POM, Unreinforced, Internally Lubricated, Ultra High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.550 - 0.600 J/cm | 1.03 - 1.12 ft-lb/in | ASTM D256 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PCC 4414 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
Solvay TECHNYL® C 52G4 MZ25 PA6, 25% mineral filler, DRY Description: TECHNYL® C 52G4 MZ25 is a 25% mineral reinforced melamine cyanurate flame retarded polyamide 6.This product is heat stabilized and is suitable for injection molding. This product is .. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM HU1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing. |
|||
Izod Impact, Notched | 0.550 J/cm @Thickness 3.20 mm |
1.03 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6520 Permanent Antistatic Polystyrene Characteristics No sloughing Fully colorable Meets MIL-PRF-81705D static decay specification Functions even in low humidity levels Processing Injection molding Extrusion & Forming Applications C.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
PlastxWorld Veroplas PA5300 Nylon 6 general purpose, 30% mineral filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature 23.0 °C |
1.03 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough PZ301R8 Polycarbonate, 40% Carbon Fiber 40% Carbon fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256A |
DSM Somos® 9110 Epoxy Photopolymer DescriptionDSM Somos® 9110 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p.. |
|||
Izod Impact, Notched | 0.550 - 0.600 J/cm | 1.03 - 1.12 ft-lb/in | ASTM D256 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Homopolymer HP0334C30L1 Calcium Reinforced |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
Carmel Olefins CAPILENE® QT 73 AV Propylene Random Copolymer Description: CAPILENE® QT 73 AV is a high melt flow rate, controlled rheology polypropylene random copolymer for injection molding of clear articles. CAPILENE® QT 73 AV is clarified with antista.. |
|||
Izod Impact, Notched | 0.550 J/cm @Temperature -30.0 °C |
1.03 ft-lb/in @Temperature -22.0 °F |
ISO 180/A |
BASF Ultraform N 2310P Q600 POM Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert.. |
|||
Izod Impact, Notched | 0.550 J/cm @Thickness 3.17 mm |
1.03 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin.. |
|||
Izod Impact, Notched | 0.550 J/cm | 1.03 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Izod Impact, Notched | 0.550 J/cm @Diameter 0.125 mm, Temperature -20.0 °C |
1.03 ft-lb/in @Diameter 0.00492 in, Temperature -4.00 °F |
bar; ASTM D256 |
BP Amoco Acctuf® 3240 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; Fiber Optic CableFeatures: NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |