Izod Impact, Notched 0.420 - 0.881 J/cm
0.787 - 1.65 ft-lb/in
Average value: 0.638 J/cm Grade Count:34
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..