Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C2100 PC+ABS (Asia Pacific) CYCOLOY C2100 is a flame retardant blend, specifically developed to meet the stringent requirements of mains current carrying applications. CYCOLOY C2100 combines |
|||
Izod Impact, Notched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Asia Pacific) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Asia Pacific) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Asia Pacific) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1132T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) .. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1162T PC Copolymer (Asia Pacific) Lexan* EXL1162T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties. This resin offers good low temperature (-20 C) ductility in c.. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL1182T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1182T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in.. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Izod Impact, Notched | 6.18 J/cm @Temperature -30.0 °C |
11.6 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXE1112T PC Copolymer (Asia Pacific) Lexan* FXE1112T Lexan* polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high flow ch.. |
|||
Izod Impact, Notched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2000U PC Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Izod Impact, Notched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2000U PC (Asia Pacific) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Izod Impact, Notched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2000U PC (Europe-Africa-Middle East) Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
Izod Impact, Notched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PRB 0131 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 6.19 J/cm | 11.6 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437C20L1 Calcium Reinforced |
|||
Izod Impact, Notched | 6.20 J/cm | 11.6 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® T80HI Impact Resistance PBT/ABS Alloy Impact ResistanceInformation provided by E-Polymers Co. Ltd. |