Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.85 J/cm @Temperature 23.0 °C |
12.8 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CE3210 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched | 6.85 J/cm | 12.8 ft-lb/in | ASTM D256 |
Kostat E-2001 Conductive PP Compound KOSTAT E-2001 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using a special conductive carbon black. In addition to a low electrical resistivity, E-200.. |
|||
Izod Impact, Notched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP) LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers. |
|||
Izod Impact, Notched | 6.83 J/cm | 12.8 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Izod Impact, Notched | 6.84 J/cm | 12.8 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® PC/ABS Alloy 306 General purpose with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |