Mechanical Properties Metric English Comments
Izod Impact, Notched 7.102 J/cm

@Thickness 3.17 mm
13.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers DIAMALOY 801 Polycarbonate/Polyester Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.