Polymer Property : Izod Impact, Notched = 13.6029 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.176 - 7.26104 J/cm

@Temperature -30.0 - 4.00 °C
0.330 - 13.6029 ft-lb/in

@Temperature -22.0 - 39.2 °F
Average value: 0.794 J/cm Grade Count:56
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..