Polymer Property : Izod Impact, Notched = 13.8 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.690 - 7.35 J/cm
1.29 - 13.8 ft-lb/in
Average value: 2.38 J/cm Grade Count:55
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..