Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.690 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GMF 604 40 UV Black 28 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003 PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific) ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Ensinger ENSIFONE® PSU (Polysulfone) - Extruded Products
(discontinued **) ENSIFONE is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. ENSIFONE is FDA and .. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
(Unverified Data**) Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY K2000 Acetal (Asia Pacific) LNP LUBRILOY* K2000 is a compound based on Acetal resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-pro.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX00887C PC LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU) Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WF006H PBT LNP* THERMOCOMP* WF006H is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 6.40 mm |
1.29 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP OF006A PPS - Branched LNP* THERMOCOMP* OF006A is a compound based on PPS - Branched resin containing 30% Glass Fiber. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 528L-5G Nylon 66, 5% Glass Reinforced General purpose glass fiber reinforced nylon, designed for parts requiring improved dimensional stability and higher strength than conventional resins.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 524 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp DCL329XZ PC (Asia Pacific) LNP LUBRICOMP* DCL329XZ is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | After Immersion in 50/50 Glycol/Water Mixture for 1,000 hours at 275°F (135°C); ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 3.20 mm |
1.29 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® MN-401 PA6 Resin Good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM AR9100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |