Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.150 - 10.0 J/cm @Temperature -40.0 - 0.000 °C |
0.281 - 18.7 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.495 J/cm Grade Count:13 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |