Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 10.00 J/cm | 18.73 ft-lb/in | ASTM D256 |
PlastxWorld Veroplas PA2002HI Nylon 6 general purpose, unfilled, high impact modified injection molding gradeInformation provided by PlastxWorld Inc. |