Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.17 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect.. |
|||
Izod Impact, Notched | 1.16 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.17 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA6-M25G20 20% Glass & 25% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 1.16 J/cm | 2.17 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON RE008 PA 66 LNP* STAT-KON* RE008 is a compound based on Nylon 66 containing 40% Carbon Fiber. Characteristics of this grade include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.16 J/cm | 2.17 ft-lb/in | ASTM D256 |
Cheng Yu Plastic A705G3 ABS 30% Glass Fiber Reinforced |
|||
Izod Impact, Notched | >= 1.16 J/cm @Thickness 6.35 mm |
>= 2.17 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |