Polymer Property : Izod Impact, Notched = 2.34 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.34 J/cm
4.38 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON DD000P PC
LNP* STAT-KON* DD000P is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Electrically Conductive, Exceptional Processing.
Izod Impact, Notched 2.34 J/cm
4.38 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific)
LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing.
Izod Impact, Notched 2.34 J/cm
4.38 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX0844 PPE+PS
PPE+PS blend. Unfilled. UL94 HB rated. Low water absorption. Hydrolytic stability. Dimensional stability.
Izod Impact, Notched 2.34 J/cm
4.38 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX0844 PPE+PS (Asia Pacific)
Automotive interiors. High heat/moisture resistant. consistant processability.
Izod Impact, Notched 2.34 J/cm
4.38 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON PX91060 PA 6
LNP* VERTON* PX91060 is a compound based on Nylon 6 resin containing Proprietary Fillers. Added feature of this grade is: Structural.
Izod Impact, Notched 2.34 J/cm
4.38 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON PX91060 PA 6 (Asia Pacific)
LNP* Verton* PX91060 is a compound based on Nylon 6 resin containing Long Glass Fiber.