Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 11.8 J/cm | 22.0 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN173HI4 High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2007 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2007F Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2007NAT Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2007UV Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2019 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2019F Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |