Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 11.7 - 11.7 J/cm @Temperature -40.0 - -40.0 °C |
21.9 - 21.9 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 11.7 J/cm Grade Count:1 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Izod Impact, Notched | 11.7 - 11.7 J/cm @Thickness 3.18 - 3.18 mm |
21.9 - 21.9 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 11.7 J/cm Grade Count:1 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2007 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2007F Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2007NAT Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2007UV Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2019 Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |
|||
Izod Impact, Notched | 11.7 J/cm | 22.0 ft-lb/in | ASTM D256 |
Colorite Polymers 2019F Rigid PVC Description: Colorite Polymers offers a wide range of rigid vinyl compounds for extrusion and injection molding applications for the medical industry. These compounds can be formulated for the produ.. |