Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 13.3 J/cm | 24.9 ft-lb/in | ASTM D256 |
IDI Composites A-207 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |