Mechanical Properties Metric English Comments
Izod Impact, Notched 3.04 J/cm
5.70 ft-lb/in
ASTM D256
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific)
ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses.
Izod Impact, Notched 3.04 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
5.69 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible
Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical
Izod Impact, Notched 3.04 J/cm
5.70 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE
LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
Izod Impact, Notched 3.04 J/cm
5.70 ft-lb/in
ASTM D256
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate
Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Izod Impact, Notched 3.04 - 4.11 J/cm
5.70 - 7.70 ft-lb/in
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound
BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding..
Izod Impact, Notched 3.04 J/cm
5.70 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific)
LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
Izod Impact, Notched 3.04 J/cm
5.70 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS
LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural.